Free fiberglass calculators for composite production planning. These tools handle the arithmetic behind everyday hand lay-up decisions: how much resin and MEKP catalyst a CSM job needs, what a multi-layer laminate weighs and how thick it cures, and how heavy a roll of fiberglass mat will be for shipping and handling.

Each calculator applies the same rules of thumb published across this site — a resin:glass ratio of 2.0–2.5:1 for hand lay-up, MEKP catalyst at 1–2% by weight for polyester and vinyl ester systems, roughly 1 mm of cured laminate per 450 g/m² CSM layer, and a cured CSM laminate density of about 1.5 g/cm³ — so the numbers you compute here match the guidance in our blog and product pages. Use them to budget resin orders, check a laminate schedule against a thickness target, or plan container loading before you request a quote. When the estimate looks right, send the results with your RFQ and we will confirm mat weight, width, roll format, MOQ from 2 tons, and lead time of 7–15 days.

Fiberglass Resin Calculator

Resin, MEKP catalyst, and laminate weight for CSM hand lay-up from mat weight, area, layers, and resin:glass ratio.

Open calculator →

Fiberglass Laminate Calculator

Stack CSM, woven roving, cloth, and surface tissue layer by layer; get glass and resin weight, fiber content, and cured thickness.

Open calculator →

Fiberglass Roll Weight Calculator

Roll weight or maximum roll length from width, length, and g/m² — for shipping, handling, and container planning.

Open calculator →