Fiberglass and Composites Glossary
A practical A-Z fiberglass glossary defining CSM, woven roving, resin systems, gel coat, LOI, Barcol hardness, and key composite terms for buyers and engineers.

A practical A-Z fiberglass glossary defining CSM, woven roving, resin systems, gel coat, LOI, Barcol hardness, and key composite terms for buyers and engineers.
Fiberglass and Composites Glossary
This fiberglass glossary defines common terms used in the fiberglass and composites industry. Use it as a quick reference when reading technical documents, comparing quotes, or talking to suppliers.
Key Takeaways
- Understanding binder terminology prevents costly resin compatibility mistakes: standard emulsion-bound CSM is not recommended for epoxy (confirm the TDS).
- Hand-lay CSM thickness follows the rule of thumb ≈1 mm per 300 g/m² ; 300 g/m² ≈ 1.0–1.3 mm, 600 g/m² ≈ 2.0–2.4 mm.
- Terms like Barcol hardness, LOI, and fiber content appear on certificates of analysis and directly indicate quality.
- Resin consumption rules of thumb (2.0–2.5× mat weight) simplify project budgeting.
- HS Code 7019.31 is the standard classification for fiberglass chopped-strand mat in international trade.
Glossary A–Z
A
Additives — Materials mixed into resin to change properties. Examples include pigments, UV stabilizers, fire retardants, and thixotropic agents.
Air Trap — A pocket of air trapped in a laminate, usually appearing as a bubble or void. Removed by rolling or vacuum.
B
Barcol Hardness — A measure of the surface hardness of a cured resin or laminate. Used to check cure completeness. Typical values range from 35 to 50 for cured polyester and vinyl ester laminates.
Binder — The material that holds chopped glass strands together in mat form. Powder binders and emulsion binders are the two main types.
Blister — A raised area on a laminate surface caused by trapped moisture, air, or solvent.
Bulk Molding Compound (BMC) — A premixed molding material containing resin, filler, and short glass fibers, used in compression and transfer molding.
C
C-Glass — A chemical-resistant glass formulation used in surface tissues and corrosion barriers for tanks and pipes.
CFM — Continuous Filament Mat. A mat made from continuous glass strands rather than chopped strands. Compatible with most resins including epoxy.
Chopped Strand Mat (CSM) — A non-woven mat made from short, randomly oriented glass fibers held together by a binder. The most common fiberglass reinforcement for hand lay-up and spray-up.
Chopper Gun — A spray-up tool that simultaneously chops glass rovings and sprays resin onto a mold.
Chop Length — The length of individual chopped glass strands in CSM, typically 25–50 mm. Shorter chops conform to complex curves; longer chops improve strength.
Corrosion Barrier — The inner, resin-rich layer of a chemical storage tank that protects structural layers from chemical attack.
Cure — The chemical reaction that converts liquid resin into a solid thermoset plastic.
D
Delamination — Separation between layers of a laminate. Usually caused by poor bonding, contamination, or impact.
Dermatitis — Skin inflammation caused by contact with uncured resin or hardener. Prevented with nitrile gloves and barrier creams.
E
E-Glass — The most common type of glass fiber for general-purpose composites, offering a balance of strength, cost, and electrical insulation.
E-CR Glass — A boron-free, corrosion-resistant glass fiber with improved acid resistance compared with standard E-glass. Used in chemical and marine applications.
Emulsion-Bound CSM — CSM held together with a water-based styrene-emulsion binder. Compatible with polyester and vinyl ester but not epoxy .
Epoxy — A thermosetting resin known for high strength, adhesion, and chemical resistance. Requires a hardener to cure.
Exotherm — Heat released during resin cure. Large resin masses can overheat and crack if not controlled.
F
Fiber Content — The percentage by weight or volume of fiber in a cured laminate. Higher fiber content usually means higher strength and stiffness.
Filament Winding — A process where continuous glass rovings are wound around a mandrel to make pipes, tanks, and pressure vessels.
Flow Media — A porous mesh or fabric placed in a vacuum infusion lay-up to help resin flow evenly through the reinforcement.
FRP — Fiber-Reinforced Plastic. A general term for composites using fiber reinforcement and a plastic matrix.
Fillers — Inert materials such as calcium carbonate or talc added to resin to reduce cost, increase viscosity, or improve properties.
G
Gel Coat — A pigmented, resin-rich surface layer applied to molds before laminating. Provides color and weather protection.
Gel Time — The time from mixing catalyst or hardener until resin becomes too thick to pour.
GMT — Glass Mat Thermoplastic. A sheet of glass mat impregnated with thermoplastic resin, used in compression molding.
Glass Transition Temperature (Tg) — The temperature above which a cured resin becomes soft and loses mechanical strength.
H
Hand Lay-up — A manual process where resin and reinforcement are applied to an open mold by hand.
Hardener — The curing agent used with epoxy resin. Mixed in a specific ratio with the base resin.
HS Code 7019.31 — The Harmonized System tariff code for fiberglass chopped-strand mats (CSM). Used for customs declarations and import/export documentation.
I
ISO Polyester — Isophthalic polyester resin. A higher-grade polyester with better water and chemical resistance than orthophthalic polyester.
Interlaminar Strength — The bonding strength between adjacent layers in a laminate. Powder-bound CSM often provides higher interlaminar strength than emulsion-bound CSM.
L
Laminate — A finished structure made of multiple layers of reinforcement and resin.
Lamination Schedule — A document specifying the sequence of reinforcements, resin types, and thicknesses for a composite part.
LOI — Loss On Ignition. A test measuring binder content in fiberglass mat by burning off the binder.
M
MEKP — Methyl Ethyl Ketone Peroxide. A common catalyst used to cure polyester and vinyl ester resins at room temperature. Typical ratio is 1–2% by volume at 20°C.
Mold — The tool or form used to shape a composite part during manufacturing.
Mold Release — A coating or wax applied to a mold surface to prevent the cured part from sticking.
O
Orthophthalic Polyester — A general-purpose, lower-cost polyester resin. Suitable for non-structural and above-waterline applications.
Osmosis — The process by which water passes through a gel coat or laminate, often leading to blistering.
P
Peel Ply — A release fabric applied to the outer layer of a laminate and peeled off after cure, leaving a textured surface ready for bonding.
Pigment — A colorant added to resin or gel coat.
Post-cure — Heating a cured laminate to an elevated temperature to improve mechanical and thermal properties.
Pot Life — The working time of a catalyzed or mixed resin before it becomes unusable.
Powder-Bound CSM — CSM held together with a thermoplastic polyester powder binder. Compatible with polyester, vinyl ester, and epoxy.
Prepreg — Reinforcement pre-impregnated with resin and partially cured, requiring refrigerated storage and heat cure.
R
Reinforcement — The fiber material in a composite that provides strength and stiffness. Glass, carbon, and aramid are common reinforcements.
Resin — The polymer matrix that binds reinforcement together and transfers load between fibers.
Resin-to-Glass Ratio — The weight ratio of resin to fiber reinforcement in a laminate. For hand-lay CSM, a typical target is 2.0:1 to 2.5:1 resin to glass by weight.
Roving — A bundle of continuous glass fibers, used as reinforcement in spray-up, pultrusion, filament winding, and woven fabrics.
RTM — Resin Transfer Molding. A closed-mold process where resin is injected into a mold containing dry reinforcement.
S
S-Glass — A high-strength glass fiber variant used in aerospace and high-performance composites.
SMC — Sheet Molding Compound. A ready-to-mold sheet of resin, glass fiber, and fillers used in compression molding.
Spray-up — A process where chopped glass and resin are sprayed onto a mold simultaneously.
Stitch-Bonded Mat — A mat held together by stitching rather than binder. Compatible with epoxy and often used in vacuum infusion.
Styrene — A reactive monomer used to thin polyester and vinyl ester resins and promote cure. Also a VOC requiring ventilation controls.
T
Tex — A unit of linear density equal to grams per 1,000 meters of fiber. Higher tex indicates thicker roving.
Thermoset — A resin that cures into a solid through a chemical reaction and cannot be remelted. Polyester, vinyl ester, and epoxy are thermosets.
Thixotropic Agent — An additive that makes resin thicker and less likely to run on vertical surfaces.
Tooling Gel Coat — A hard, durable gel coat used on molds rather than finished parts.
U
UV Resistance — The ability of a material to resist degradation from ultraviolet light. Gel coats and resins often include UV stabilizers.
V
Vacuum Infusion — A process where resin is pulled through dry reinforcement using vacuum pressure inside a sealed bag.
Vinyl Ester — A thermosetting resin with excellent chemical resistance and toughness. Often used in chemical storage and marine applications.
Void — An empty space or bubble in a laminate that reduces strength and can allow moisture ingress.
Volatile Organic Compounds (VOCs) — Organic chemicals that evaporate during resin cure. Styrene is the main VOC in polyester and vinyl ester systems.
W
Wet-out — The process of saturating reinforcement with resin so that all fibers are coated and air is displaced.
Woven Roving — A heavy fabric made from continuous glass fibers woven in a simple over-under pattern. Provides high strength and stiffness.
Common Mistakes When Reading Specifications
❌ Confusing Weight and Thickness
- Problem: Assuming 300 g/m² and 600 g/m² produce the same cured thickness.
- Solution: Use the rule of thumb ≈1 mm of cured thickness per 300 g/m² of CSM . 300 g/m² ≈ 1.0–1.3 mm, 600 g/m² ≈ 2.0–2.4 mm. Vacuum-bagged or press-molded parts are thinner.
❌ Ignoring Binder Compatibility
- Problem: Ordering emulsion-bound CSM for an epoxy project.
- Solution: Specify powder-bound CSM or stitch-bonded mat for epoxy systems.
❌ Misreading Resin Consumption
- Problem: Budgeting 1:1 resin to glass.
- Solution: Plan on 2.0–2.5 kg resin per kg CSM by weight.
❌ Overlooking Test Standards
- Problem: Not requesting Barcol hardness or LOI values.
- Solution: Ask suppliers for test reports aligned with ASTM or ISO standards.
Quick Reference Tables
Core Terminology
| Term | Definition | Why It Matters |
|---|---|---|
| CSM | Chopped strand mat | Most common hand-lay reinforcement |
| LOI | Binder content by burn-off | Indicates binder type and amount |
| Barcol Hardness | Surface hardness of cured resin | Confirms full cure |
| MEKP | Catalyst for polyester/vinyl ester | Typical 1–2% at 20°C |
| Tg | Glass transition temperature | Limits maximum service temperature |
| HS 7019.31 | Tariff code for CSM | Required for import/export |
Binder and Resin Compatibility
| Binder Type | Compatible Resins | Not Compatible With | Best For |
|---|---|---|---|
| Powder-bound CSM | Polyester, vinyl ester, epoxy | — | General purpose and epoxy work |
| Emulsion-bound CSM | Polyester, vinyl ester | Epoxy | Cost-sensitive polyester/vinyl ester jobs |
| Stitch-bonded mat | Polyester, vinyl ester, epoxy | — | Vacuum infusion and large structures |
Quick Decision Checklist
When Reviewing a Fiberglass Specification
- CSM weight matches target laminate thickness (≈1 mm per 300 g/m² for hand lay-up)
- Binder type matches resin system (powder or stitch-bonded for epoxy)
- Resin consumption is budgeted at 2.0–2.5× CSM weight
- MEKP ratio is 1–2% for polyester/vinyl ester at 20°C
- Quality tests (Barcol, LOI, weight uniformity) are documented
- HS Code 7019.31 is noted for international orders
- Gel coat and UV protection are specified for outdoor parts
- Post-cure requirements are included for high-temperature service
FAQ: Fiberglass and Composites Glossary
Q1: What is the difference between CSM and woven roving?
A: CSM consists of randomly oriented chopped strands held by binder, making it conformable and ideal for building thickness. Woven roving consists of continuous fibers woven in a pattern, providing higher strength in specific directions.
Q2: Why is binder type so important?
A: The binder determines resin compatibility. Standard emulsion-bound CSM is not recommended for epoxy (confirm the TDS), while powder-bound CSM works with polyester, vinyl ester, and epoxy.
Q3: What does HS Code 7019.31 mean?
A: HS Code 7019.31 is the international customs classification for fiberglass chopped-strand mats. It is used on shipping documents, invoices, and customs declarations.
Q4: How is LOI used in quality control?
A: LOI (Loss on Ignition) measures the percentage of binder in CSM by burning it off. Typical values are 4–8%, depending on binder type and application.
Q5: What Barcol hardness value indicates a fully cured laminate?
A: For most polyester and vinyl ester laminates, a Barcol hardness above 35 indicates adequate cure. Higher values (40–50) indicate fuller cure and better surface hardness.
Data Sources and Verification
Thickness, Resin, and Process Data
- CSM weight-to-thickness estimate (≈1 mm per 300 g/m²): industry rule of thumb for hand-lay laminates with typical resin content; vacuum-bagged or press-molded laminates are thinner.
- Resin-to-glass ratio 2.0–2.5:1: industry experience for hand-lay CSM; actual ratio varies by process and compaction.
- MEKP 1–2% by volume at 20°C: typical resin supplier recommendation for room-temperature cure of polyester and vinyl ester resins.
Trade and Testing References
- HS Code 7019.31: World Customs Organization harmonized system classification for fiberglass chopped-strand mats.
- Barcol hardness values: based on ASTM D2583 test method for rigid plastics.
Need Fiberglass Mat for Your Project?
We supply high-quality CSM, CFM, and specialty fiberglass products worldwide. Custom specifications available with low MOQ.
Request Free QuoteView Products
PrimeMat
Leading manufacturer of chopped strand mat and continuous filament mat for industrial applications. ISO 9001 certified with 15+ years experience.
Request a quote
We can manufacture fiberglass mat to your exact requirements.
- ISO 9001 certified production
- Reply within 24 hours (EN / ZH)
- Or WhatsApp +86 138 1403 4409