Fiberglass Unit Conversion Tables
Quick reference fiberglass conversion tables for weight per area, thickness, density, temperature, pressure, resin consumption, and fiber content for engineers.

Quick reference fiberglass conversion tables for weight per area, thickness, density, temperature, pressure, resin consumption, and fiber content for engineers.
Fiberglass Unit Conversion Tables
Use these fiberglass conversion tables to convert between common units used in the fiberglass and composites industry. These conversions help estimators, buyers, and engineers translate supplier specs, drawings, and purchase orders quickly.
Key Takeaways
- Hand-lay CSM cures to approximately 1 mm of total thickness per 300 g/m² of mat : 300 g/m² ≈ 1.0–1.3 mm, 450 g/m² ≈ 1.5–1.8 mm, 600 g/m² ≈ 2.0–2.4 mm.
- Resin consumption is typically 2.0–2.5 times the CSM weight by area (the resin-to-glass ratio).
- Weight-per-area conversions: g/m² × 0.0295 = oz/yd²; oz/yd² × 33.9 = g/m².
- MEKP catalyst for polyester and vinyl ester is typically 1–2% by volume at 20°C.
- HS Code 7019.31 classifies fiberglass chopped-strand mat for international trade.
Weight and Area Conversions
Weight per Area
| g/m² | oz/yd² | lb/ft² |
|---|---|---|
| 100 | 2.95 | 0.0205 |
| 225 | 6.64 | 0.0461 |
| 300 | 8.85 | 0.0614 |
| 450 | 13.28 | 0.0922 |
| 600 | 17.70 | 0.1229 |
| 900 | 26.55 | 0.1843 |
To convert g/m² to oz/yd²: multiply by 0.0295. To convert oz/yd² to g/m²: multiply by 33.9.
The oz Trap: oz/ft² (Mat) vs oz/yd² (Cloth) — a 9× Difference
The table above assumes oz/yd², which is how woven cloth and roving are labeled. But in North America, chopped strand mat is labeled in ounces per square FOOT. The two conventions differ by exactly 9× (1 yd² = 9 ft²), so a "1.5 oz" mat and a "1.5 oz" cloth are not the same weight per area — not even close:
| Label | Convention | Actual weight |
|---|---|---|
| 1.5 oz CSM | oz per ft² | 1.5 × 305.2 = ≈458 g/m² (matches 450 g/m² metric CSM) |
| 1.5 oz woven cloth | oz per yd² | 1.5 × 33.9 = ≈51 g/m² |
| 0.75 oz CSM | oz per ft² | ≈229 g/m² (matches 225 g/m² metric CSM) |
| 6 oz cloth | oz per yd² | ≈203 g/m² |
Conversion factors: 1 oz/ft² = 305.2 g/m²; 1 oz/yd² = 33.9 g/m²; ratio = 9.0.
This is the single most common quantity-ordering mistake in fiberglass purchasing: buyers converting mat weights with the cloth factor under-order by a factor of nine. When a US-market repair guide calls for "1.5 oz mat", it means the ~450 g/m² product — the standard hand-lay weight for hull repairs — while "2 oz cloth" is a light ~68 g/m² surface fabric. When requesting quotes across markets, always state the convention explicitly (e.g., "450 g/m² (1.5 oz/ft²)") or check the g/m² figure first; metric-labeled CSM from international suppliers sidesteps the ambiguity entirely.
Roll Length and Area Conversions
CSM is typically supplied in rolls. Use these conversions to check delivered quantities.
| Roll Width (m) | Roll Length (m) | Roll Area (m²) | Roll Area (ft²) |
|---|---|---|---|
| 1.0 | 100 | 100 | 1,076 |
| 1.27 | 100 | 127 | 1,367 |
| 1.5 | 100 | 150 | 1,615 |
| 2.0 | 100 | 200 | 2,153 |
To convert square meters to square feet, multiply by 10.764.
Thickness and Density Conversions
CSM Weight to Thickness (Approximate)
| CSM Weight (g/m²) | Cured Thickness (mm) | Cured Thickness (in) |
|---|---|---|
| 300 | 1.0–1.3 | 0.039–0.051 |
| 450 | 1.5–1.8 | 0.059–0.071 |
| 600 | 2.0–2.4 | 0.079–0.094 |
| 900 | 3.0–3.6 | 0.118–0.142 |
Rule of thumb: approximately 1 mm per 300 g/m² for hand-lay CSM. Vacuum-bagged, infused, or press-molded laminates are thinner due to higher compaction.
Thickness Conversion Table
| mm | in | mils |
|---|---|---|
| 0.5 | 0.020 | 20 |
| 1.0 | 0.039 | 39 |
| 1.5 | 0.059 | 59 |
| 2.0 | 0.079 | 79 |
| 3.0 | 0.118 | 118 |
| 4.0 | 0.157 | 157 |
| 5.0 | 0.197 | 197 |
| 6.0 | 0.236 | 236 |
One mil equals 0.001 inch.
Density
| Material | kg/m³ | lb/ft³ |
|---|---|---|
| E-glass fiber | 2,540 | 158.6 |
| Cured polyester/CSM | 1,400–1,600 | 87–100 |
| Cured vinyl ester/CSM | 1,450–1,650 | 90–103 |
| Cured epoxy/glass | 1,500–1,700 | 94–106 |
Resin and Fiber Calculations
Resin Consumption
| CSM Weight (g/m²) | Resin Needed (g/m²) | Resin Needed (oz/ft²) |
|---|---|---|
| 300 | 600–750 | 1.96–2.45 |
| 450 | 900–1,125 | 2.94–3.68 |
| 600 | 1,200–1,500 | 3.92–4.90 |
| 900 | 1,800–2,250 | 5.89–7.36 |
Rule of thumb: 2.0–2.5 kg resin per kg of CSM (resin-to-glass ratio by weight).
Resin-to-Fiber Ratio by Weight
| Ratio (Resin:Fiber) | Fiber Weight Fraction | Fiber Volume Fraction (E-glass) | Typical Process |
|---|---|---|---|
| 1.5:1 | 40% | ~25% | Vacuum infusion |
| 2.0:1 | 33% | ~20% | Vacuum bagging |
| 2.5:1 | 29% | ~17% | Hand lay-up with CSM |
| 3.0:1 | 25% | ~15% | Open mold, resin-rich |
Lower ratios are lighter and stronger but require better consolidation.
Fiber Content Conversion
| Fiber Weight Fraction | Fiber Volume Fraction (E-glass, polyester) |
|---|---|
| 20% | ~11% |
| 30% | ~18% |
| 40% | ~25% |
| 50% | ~33% |
| 60% | ~42% |
Process Parameter Conversions
Temperature
| °C | °F |
|---|---|
| 10 | 50 |
| 20 | 68 |
| 25 | 77 |
| 50 | 122 |
| 80 | 176 |
| 100 | 212 |
| 120 | 248 |
| 150 | 302 |
Formula: °F = (°C × 9/5) + 32. Formula: °C = (°F − 32) × 5/9.
Pressure
| Unit | 1 bar equals |
|---|---|
| psi | 14.5 |
| kPa | 100 |
| MPa | 0.1 |
| atm | 0.987 |
Catalyst Ratio Reference
For polyester and vinyl ester resins cured with MEKP at approximately 20°C:
| Catalyst % | Per 1 kg Resin | Per 1 gallon Resin (~4 kg) | Typical Use Case |
|---|---|---|---|
| 1% | 10 g / 8.5 ml | 40 g / 34 ml | Hot weather, long working time |
| 1.5% | 15 g / 12.8 ml | 60 g / 51 ml | Standard room temperature |
| 2% | 20 g / 17.1 ml | 80 g / 68 ml | Cold weather, faster cure |
Note: MEKP density is approximately 1.17 g/ml. Catalyst ratio should be adjusted for temperature: reduce in hot weather, increase in cold weather, but generally keep within 1–2%.
Using These Tables in Quotations and Specifications
Specifying Units in RFQs
When preparing a request for quotation, include the conversions your suppliers should use. For example, state that CSM weight is specified in g/m², thickness is estimated using the rule of thumb ≈1 mm per 300 g/m² , and resin consumption is budgeted at 2.0–2.5 times the mat weight. This reduces disputes over unit interpretation and ensures quotes are comparable. Always ask suppliers to confirm the HS Code 7019.31 for international shipments and to report roll dimensions in both metric and imperial units if your drawings use mixed units.
Practical Calculation Examples
Example 1: Estimating CSM for a Boat Hull
A hull panel measures 5 m × 2 m and requires 4 mm total thickness. Using 450 g/m² CSM (≈1.5–1.8 mm per layer for hand lay-up):
- Surface area: 5 × 2 = 10 m²
- Layers needed: 4 mm ÷ ~1.65 mm per layer ≈ 2.4 → use 3 layers for 4.5–5.4 mm total
- CSM required: 10 m² × 3 layers × 1.2 (waste/overlap) = 36 m²
- Resin required: 36 m² × 450 g/m² × 2.25 = 36.45 kg
Example 2: Converting Supplier Specs
A supplier quotes 1.5 oz/yd² CSM. Convert to g/m²:
- 1.5 oz/yd² × 33.9 = 50.85 g/m²
- In practice, many suppliers use the approximate convention 1.0 oz/yd² ≈ 300 g/m² for CSM. Always confirm whether the quote uses exact conversion or industry convention before ordering.
Example 3: Catalyst Measurement
For 2 kg of polyester resin at 20°C with 1.5% MEKP:
- 2,000 g × 0.015 = 30 g MEKP
- MEKP density ≈ 1.17 g/ml, so 30 g ≈ 25.6 ml
Common Conversion Mistakes
❌ Confusing oz/yd² with oz/ft²
- Problem: Using the wrong conversion factor.
- Solution: Remember 1 oz/yd² = 33.9 g/m²; 1 oz/ft² = 305 g/m².
❌ Ignoring Waste and Overlap
- Problem: Ordering exact surface area without overlap.
- Solution: Add 15–20% for seams, trim, and handling waste.
❌ Assuming All CSM Weights Have the Same Thickness
- Problem: Thinking 300 g/m² and 600 g/m² produce equal thickness per layer.
- Solution: Use the rule of thumb ≈1 mm of cured thickness per 300 g/m² of CSM for hand-lay estimates.
❌ Forgetting Resin-to-Glass Ratio
- Problem: Budgeting equal weights of resin and CSM.
- Solution: Plan on 2.0–2.5 kg resin per kg CSM.
Quick Decision Checklist
When Estimating a Fiberglass Project
- All weights are converted to a consistent unit (prefer g/m²)
- Thickness targets are translated to CSM weight using ≈1 mm per 300 g/m²
- Number of layers accounts for 15–20% overlap/waste
- Resin quantity is 2.0–2.5× total CSM weight
- MEKP catalyst is calculated at 1–2% by volume
- Temperature units are consistent across resin datasheets
- Fiber content target is defined and testable
- HS Code 7019.31 is recorded for international CSM shipments
FAQ: Fiberglass Conversion Tables
Q1: How many grams per square meter is 1 ounce per square yard?
A: 1 oz/yd² = 33.9 g/m². In the fiberglass industry, 1.0 oz/yd² is often approximated as 300 g/m² for practical CSM specification, but the exact conversion is 33.9 g/m² per ounce.
Q2: How thick is 600 g/m² CSM after curing?
A: Approximately 2.0–2.4 mm (0.079–0.094 in) using the rule of thumb ≈1 mm per 300 g/m² . Actual thickness depends on resin content, rolling pressure, and compaction.
Q3: How much resin do I need for 10 m² of 450 g/m² CSM?
A: The CSM weighs 10 × 450 = 4,500 g. At 2.0–2.5× resin-to-glass ratio, you need 9.0–11.25 kg of resin. Add 10% waste for mixing and touch-ups.
Q4: What is the HS Code for fiberglass chopped-strand mat?
A: HS Code 7019.31 is the international classification for fiberglass chopped-strand mats used in customs and trade documentation.
Q5: How do I convert Barcol hardness units?
A: Barcol hardness is reported on a Barcol scale (e.g., 934-1 or 935). Values above 35 typically indicate adequate cure for marine laminates. Always compare readings using the same Barcol impressor model.
Data Sources and Verification
Unit and Conversion Factors
- Weight-per-area conversions: exact factors are 1 oz/yd² = 33.9057 g/m² and 1 oz/ft² = 305.152 g/m²; rounded values are used for practical estimation.
- CSM weight-to-thickness estimate (≈1 mm per 300 g/m²): industry rule of thumb for hand-lay laminates; vacuum infusion, vacuum bagging, and press molding produce thinner laminates.
Process and Trade References
- Resin consumption 2.0–2.5× CSM weight: typical resin-to-glass ratio for hand-lay CSM; verify against your resin supplier's data sheet.
- MEKP density ~1.17 g/ml and catalyst ratio 1–2% at 20°C: typical supplier recommendations for room-temperature cure of polyester and vinyl ester resins.
- HS Code 7019.31: World Customs Organization harmonized system classification for fiberglass chopped-strand mats.
Need Fiberglass Mat for Your Project?
We supply high-quality CSM, CFM, and specialty fiberglass products worldwide. Custom specifications available with low MOQ.
Request Free QuoteView Products
PrimeMat
Leading manufacturer of chopped strand mat and continuous filament mat for industrial applications. ISO 9001 certified with 15+ years experience.
Request a quote
We can manufacture fiberglass mat to your exact requirements.
- ISO 9001 certified production
- Reply within 24 hours (EN / ZH)
- Or WhatsApp +86 138 1403 4409