Chopped Strand Mat Data Sheet: How to Read Specifications & COA
Learn how to read a chopped strand mat data sheet. Understand mass per unit area, LOI, moisture, tensile strength, and binder type for better procurement.

Learn how to read a chopped strand mat data sheet. Understand mass per unit area, LOI, moisture, tensile strength, and binder type for better procurement.
Chopped Strand Mat Data Sheet: How to Read Specifications & COA
This guide explains every field on a chopped strand mat data sheet (TDS) and certificate of analysis (COA). For a broader buying overview, see our Fiberglass Mat Buyer's Guide . A chopped strand mat specification sheet is the most important document for comparing suppliers and verifying that a CSM roll meets your requirements. Every number on the sheet — weight, binder content, moisture, tensile strength — directly affects how the mat will perform in your process and in the final part.
This guide explains the key parameters found on a CSM data sheet, what each number means, how to spot red flags, and how to use the sheet to write a clear purchase order. It is written for procurement managers, quality engineers, and shop supervisors who need to evaluate CSM before buying. Learning to read a chopped strand mat specification properly can save you from costly batch rejections and production delays.
Why Reading a Chopped Strand Mat Data Sheet Matters
The Cost of Ignoring Specifications
Many CSM quality problems can be traced back to unverified or misunderstood data sheets. Reading the chopped strand mat specification carefully before ordering is the first line of defense. A batch with high weight variation creates thickness inconsistencies. High moisture content causes blistering and poor cure. The wrong binder type makes the mat incompatible with your resin system.
| Problem | Common Data Sheet Cause |
|---|---|
| Thickness inconsistency | Weight variation ±10% or more |
| Blisters in laminate | Moisture content >0.2% |
| Poor wet-out | Wrong binder type or excessive LOI |
| Weak laminate | Low tensile strength or damaged fibers |
| Resin incompatibility | Emulsion binder specified for epoxy use |
| Color variation | Inconsistent fiber sizing or binder |
What a Good Data Sheet Tells You
A complete CSM data sheet should define the product, state the test methods used, give typical values with acceptable ranges, and provide a certificate of analysis (COA) for each batch. If any of these elements are missing, the supplier may not have adequate quality control. Always ask for clarification before committing to an order.
A data sheet is not a marketing document. It is a technical contract that tells you whether the material will work in your process. Treat it accordingly. Two suppliers may both list "450 g/m² CSM," but the actual products can differ significantly in consistency, binder quality, and handling.
Key Parameters on a CSM Data Sheet
Parameters to Review
| Parameter | Meaning | Typical Value | Why It Matters |
|---|---|---|---|
| Mass per unit area | Weight per square meter | 225-900 g/m² | Determines thickness and strength |
| Loss on ignition (LOI) | Binder content by weight | 2-8% | Affects wet-out and bond |
| Moisture content | Water in the mat | <0.2% | Affects cure and blistering |
| Width deviation | Roll width tolerance | ±5 mm | Affects lay-up efficiency |
| Tensile strength | Strength of cured laminate | 80-120 MPa | Load-bearing capacity |
| Styrene solubility | How fast binder dissolves | <60s powder, <120s emulsion | Process speed |
| Binder type | Emulsion / powder / stitch | Listed explicitly | Resin compatibility |
| Fiber type | E-glass / ECR-glass / C-glass | Listed explicitly | Chemical resistance |
| Roll weight / length | How much material per roll | 30-80 kg | Logistics and handling |
| Chop length | Length of glass strands | 25-50 mm | Wet-out and conformability |
How to Interpret Each Parameter
Mass Per Unit Area (Weight)
Mass per unit area is the weight of one square meter of dry mat. It is measured per ISO 3374. A 450 g/m² CSM means each square meter weighs 450 grams before resin is applied.
| Weight Tolerance | Interpretation |
|---|---|
| ±5% | Industry standard, acceptable |
| ±8% | Marginal, may cause thickness issues |
| ±10% or more | Poor quality control, reject |
High weight variation across a roll means some areas will be thicker or thinner than designed. This is especially problematic for parts with tight thickness tolerances. For example, a boat hull designed with 450 g/m² CSM could end up with local thickness variations of 0.2 mm or more if the weight tolerance is poor. In a large hull, this adds weight, affects fairness, and can create weak spots.
Loss on Ignition (LOI)
LOI represents the percentage of material burned off when a sample is heated to high temperature. For CSM, this is essentially the binder content.
| Binder Type | Typical LOI |
|---|---|
| Powder-bound | 3-5% |
| Emulsion-bound | 5-8% |
| Stitch-bonded | 0-2% |
LOI that is too high indicates excessive binder, which can slow wet-out and reduce interlaminar bond strength. LOI that is too low may mean insufficient binder, causing the mat to fall apart during handling.
When you see an LOI value, compare it to the binder type claimed on the data sheet. An emulsion-bound CSM with LOI below 5% may have been mislabeled. A powder-bound CSM with LOI above 6% may have excess binder that will slow wet-out.
Moisture Content
Moisture content must be below 0.2% for most polyester and vinyl ester systems. Higher moisture can interfere with resin cure, cause bubbling, and reduce mechanical properties.
| Moisture Level | Effect |
|---|---|
| <0.2% | Acceptable |
| 0.2-0.5% | Risk of blisters and weak cure |
| >0.5% | Likely to cause significant defects |
Moisture is particularly problematic in humid climates or when rolls are stored without proper moisture barriers. Always check the packaging condition on arrival, not just the data sheet. Water stains, torn PE film, or musty odors are signs that moisture may have entered the roll.
Tensile Strength
Tensile strength on a CSM data sheet usually refers to the cured CSM/polyester laminate, tested per ASTM D638. Typical values range from 80 to 120 MPa for 450 g/m² CSM.
When comparing suppliers, make sure both data sheets use the same resin system and test standard. A value measured with epoxy will be higher than one measured with polyester. If the data sheet does not specify the resin and test method, the number is not directly comparable and should not be used for supplier selection.
Styrene Solubility
Styrene solubility measures how quickly the mat disperses in styrene. It is a practical indicator of wet-out speed.
| Binder Type | Typical Solubility |
|---|---|
| Powder-bound | <60 seconds |
| Emulsion-bound | <120 seconds |
Slower solubility is not necessarily bad, but it should match your process requirements. Fast-cycling production lines usually prefer powder-bound CSM. Hand lay-up operations may tolerate either binder type with polyester or vinyl ester resin.
Binder Type and Fiber Type
These two parameters determine resin compatibility and chemical resistance. The binder type must match your resin system. The fiber type must match the chemical environment.
| Your Resin | Required Binder |
|---|---|
| Polyester | Emulsion, powder, or stitch |
| Vinyl ester | Emulsion, powder, or stitch |
| Epoxy | Powder or stitch only |
| Environment | Recommended Fiber |
|---|---|
| General purpose | E-glass |
| Chemical service | ECR-glass or C-glass |
| High temperature | ECR-glass or S-glass |
Roll Weight and Length
Roll weight and length help you plan handling, pallet counts, and container loads. A 450 g/m² CSM roll that is 1.27 m wide and 100 m long weighs approximately 57 kg. Check that your lifting equipment, rack width, and unwinding station can handle the specified roll dimensions.
Roll weight (kg) = Weight (g/m²) × Width (m) × Length (m) ÷ 1000 Confirm that the roll weight matches your handling equipment and that the length is consistent with your production planning.
Red Flags — What to Watch Out For
Common Specification Red Flags
| Red Flag | What It Means |
|---|---|
| Missing LOI value | Binder content is uncontrolled |
| Missing moisture content | Drying process may be inadequate |
| "Typical" values without ranges | Actual variation may be large |
| No test standard listed | Values cannot be verified |
| Weight without ±% tolerance | Actual weight may vary widely |
| No COA offered | Batch traceability is poor |
| Inconsistent units | Supplier may be mixing data sources |
| Claims without test method | Marketing language, not technical data |
If you see two or more of these red flags on the same data sheet, request more information before ordering. A reputable supplier will be able to provide complete data and test reports without delay.
Certificate of Analysis and Data Sheet
Certificate of Analysis (COA) vs Data Sheet
A chopped strand mat data sheet describes the product design: typical values, test methods, and acceptance ranges. A certificate of analysis (COA) is a batch-specific document that reports the actual measured values for the roll or lot you are buying.
| Document | Scope | Updates | Use Case |
|---|---|---|---|
| Data sheet / TDS | Product design | Rarely | Supplier qualification, specification writing |
| COA | Specific batch | Every batch | Incoming inspection, batch traceability, dispute resolution |
Always request both documents. The data sheet tells you what the product should be; the COA tells you what the batch actually is. If the COA values drift outside the data sheet ranges, the material should be quarantined until the supplier explains the deviation.
Reading the COA
A COA is only useful if you can verify that it describes the rolls on your receiving dock. This section covers the fields a complete COA must include, how to check each reported value against your specification, and when a batch should be rejected.
Required COA Fields
A complete COA for fiberglass mat should contain:
- Supplier name and contact information
- Product description and grade
- Batch or lot number
- Date of manufacture and testing
- Weight per unit area
- Binder type and LOI value
- Moisture content
- Glass type
- Tensile or mechanical test results (if applicable)
- Test method references
- Authorized signature
If any of these items are missing, ask the supplier to complete the document. A COA without a batch number cannot be tied to the rolls on your receiving dock, and a COA without test method references cannot be independently verified.
Verifying Weight Per Area
Weight per area is the first property to check because it determines laminate thickness, resin consumption, and part cost. Compare the reported value to your specification tolerance:
| Nominal Weight | Typical Tolerance |
|---|---|
| 225-600 g/m² | ±5% |
| >600 g/m² | ±4% |
A 450 g/m² roll should test between 427 and 472 g/m². Values outside this range indicate a manufacturing issue. Weight deviation has direct cost consequences: hand-lay CSM thickness is roughly 1 mm per 300 g/m², and resin consumption is typically 2.0-2.5 times the mat weight, so a batch that is 5% heavy will consume roughly 5% more resin than planned.
Comparing Values to Your Specification
For each incoming batch, record the COA values against your acceptance criteria:
| Property | Your Spec | COA Value | Pass/Fail |
|---|---|---|---|
| Weight | 450 ±5% | 462 g/m² | Pass |
| LOI | 4-6% | 4.8% | Pass |
| Moisture | <0.2% | 0.12% | Pass |
| Tensile | >80 MPa | 95 MPa | Pass |
Apply the interpretation rules from the parameter sections above: moisture should be below 0.2% for most applications and below 0.1% for high-performance or epoxy systems, LOI must match the declared binder type, and tensile results are only comparable when the COA states the resin system and test method used. Keep the completed table with the batch record; over time, the trend data will reveal whether a supplier is drifting toward specification limits.
Red Flags in COAs
| Red Flag | What It Means |
|---|---|
| Missing batch number | Poor traceability |
| No test method references | Values cannot be verified |
| Wrong units | Possible data error |
| Inconsistent batch numbers across documents | Documentation mix-up |
| Values outside normal ranges | Potential quality issue |
| No signature or authorization | Document may not be official |
Also watch for COA dates that predate the manufacturing date, photocopied signatures, or test results that look identical across multiple batches. These indicate copy-paste documentation rather than actual testing.
When to Reject a Batch
Reject a batch when:
- Weight per area is outside tolerance
- LOI does not match the specified binder type
- Moisture content exceeds your maximum
- Mechanical properties fail to meet minimum requirements
- Documentation is incomplete or inconsistent
- Batch number does not match the physical roll labels
Document every rejection and communicate it to the supplier with specific reasons. Include the COA in question, highlight the out-of-spec values, and state whether you require replacement material, a refund, or a deviation approval for limited use.
A Sample CSM Specification Sheet
Example Data Sheet Layout
The following table shows how a well-structured CSM data sheet might look. This is a generic example for reference only.
| Parameter | Specification | Test Method |
|---|---|---|
| Product name | E-glass chopped strand mat, powder-bound | — |
| Weight | 450 g/m² ±5% | ISO 3374 |
| Width | 1,270 mm ±5 mm | — |
| LOI | 3.5-4.5% | ISO 1887 |
| Moisture content | <0.2% | ISO 3344 |
| Tensile strength | 90-110 MPa | ASTM D638 |
| Styrene solubility | <60 seconds | Internal method |
| Binder type | Powder | — |
| Fiber type | E-glass | — |
| Roll weight | 50-60 kg | — |
Use this structure as a template when requesting specifications from suppliers. Ask the supplier to fill in their values and confirm that each parameter is tested on every production batch.
How to Use a Chopped Strand Mat Data Sheet in Procurement
Step 1 — Create Your Internal Specification
Before contacting suppliers, define your requirements:
- Target weight and tolerance
- Binder type based on resin system
- Fiber type based on chemical environment
- Maximum moisture content
- Required test standards
- Roll dimensions and packaging
Step 2 — Request Data Sheets and COAs
Ask each supplier for the product data sheet and a recent COA. Compare them against your internal specification.
Step 3 — Write a Clear Purchase Order
Include the key parameters in the purchase order:
CSM 450 g/m² ±5%, E-glass, powder-bound, width 1,270 mm ±5 mm, moisture <0.2%, LOI 3-5%, with COA per shipment.
Step 4 — Inspect Incoming Material
When the material arrives, check the packaging, label, and visual appearance. Cut a sample and verify weight if you have the equipment. Compare the COA to your purchase order.
What You Should Do Now
Procurement Action Plan
- Collect data sheets from all potential suppliers. Do not rely on verbal claims or previous experience alone.
- Compare parameters side by side. Use the same units and test methods. If methods differ, ask suppliers to provide values using your preferred standard.
- Check for red flags. Missing data, wide tolerances, and absent test standards are warning signs.
- Request a certificate of analysis. A COA confirms that the specific batch you are buying meets the specification.
- Order samples for testing. Run a trial laminate with your resin and process before placing a large order.
- Write specifications into the purchase order. Include weight, binder type, fiber type, tolerances, test methods, and COA requirements for every chopped strand mat data sheet you reference. For help interpreting specifications, contact PrimeMat through the quote request page .
Data Sources & Verification
Sources and Standards
- Mass per unit area measurement: ISO 3374 standard test method.
- Loss on ignition (LOI): ISO 1887 standard test method for glass fiber products.
- Moisture content: ISO 3344 standard test method for glass fiber moisture.
- Tensile strength: ASTM D638 standard test method for reinforced plastics.
- Styrene solubility: common industry practice, often based on internal supplier methods.
- Typical CSM mechanical properties: representative values for CSM/polyester laminates; actual values vary with resin, cure, and test conditions.
Keep this chopped strand mat data sheet guide on hand when qualifying suppliers, and request a COA before accepting each shipment.
Need Fiberglass Mat for Your Project?
We supply high-quality CSM, CFM, and specialty fiberglass products worldwide. Custom specifications available with low MOQ.
Request Free QuoteView Products
PrimeMat
Leading manufacturer of chopped strand mat and continuous filament mat for industrial applications. ISO 9001 certified with 15+ years experience.
Request a quote
We can manufacture fiberglass mat to your exact requirements.
- ISO 9001 certified production
- Reply within 24 hours (EN / ZH)
- Or WhatsApp +86 138 1403 4409