Technical guide

Automotive RTM Case Study: Hand Lay-up to RTM Switch

Automotive RTM case study: how a Tier-2 supplier switched from hand lay-up to RTM, raised output 300%, cut scrap 60%, and recovered tooling cost in 14 months.

Automotive RTM Case Study: Hand Lay-up to RTM Switch | PrimeMat
Automotive RTM Case Study: Hand Lay-up to RTM Switch | PrimeMat

Automotive RTM case study: how a Tier-2 supplier switched from hand lay-up to RTM, raised output 300%, cut scrap 60%, and recovered tooling cost in 14 months.

Disclosure: This case study is a representative example based on typical project outcomes in this industry. Figures are rounded and illustrative; identifying details are omitted.

Automotive RTM Case Study: Hand Lay-up to RTM Switch

Executive Summary

At a Glance

This automotive RTM case study follows a Tier-2 supplier producing under-body shields that switched from open-mold hand lay-up to Resin Transfer Molding (RTM). The move increased monthly output from 150 to 600 parts, reduced scrap from 12% to 5%, and cut labor hours per part by 56%. The project paid back its tooling investment in 14 months. Key success factors were powder-bound reinforcements, proper venting, heated molds, and structured operator training.

Case Background: Automotive RTM Case Study

Before the Switch

An automotive Tier-2 supplier produced under-body shields for light commercial vehicles using open-mold hand lay-up. The process required operators to cut reinforcements by hand, apply resin, and roll each layer into the mold. Output was limited to about 150 parts per month on a single shift.

Quality and Capacity Constraints

Part-to-part variation was significant. Thickness varied by ±15%, and surface quality was inconsistent. Each part required 30 to 45 minutes of trimming, sanding, and filling after demolding. Scrap rate was 12%, driven by dry spots, resin-rich edges, and damaged gel coat.

When the OEM customer increased the contract to 500 parts per month, the supplier realized that hand lay-up could not meet the volume or quality requirements without a major increase in labor and floor space.

Decision to Switch

Process Alternatives Evaluated

The supplier evaluated three alternatives:

  • Spray-up : faster than hand lay-up but lower fiber content and rougher surfaces.
  • Compression molding with SMC : excellent surface quality and fast cycle times, but tooling cost was high for the projected volume.
  • Resin Transfer Molding : good surface on both sides, moderate tooling cost, and better dimensional control than spray-up.

Why RTM Won

RTM was selected because it offered the best balance of tooling investment, part quality, and scalability. The projected payback period was 14 months based on labor savings and scrap reduction.

Implementation

Mold and Equipment Investment

The supplier invested approximately $40,000 in matched aluminum molds and a low-pressure resin injection unit. The mold was designed with:

  • A perimeter seal groove for consistent closure.
  • Multiple injection gates to control flow front progression.
  • Vacuum vents at the last points to fill.
  • Heating channels to maintain 45°C mold temperature.

Process Parameters

The laminate stack used powder-bound continuous filament mat and chopped strand mat with a vinyl ester resin. Process parameters were:

ParameterValue
Mold temperature45°C
Resin temperature35°C
Injection pressure2-3 bar
Cure time25 minutes
Fiber content target38% by weight
Demold time35 minutes

Training and Process Tuning

Operators received two weeks of training on mold closure, clamping pressure, injection timing, vent monitoring, and demolding. The first production week was used for process tuning, during which fiber content and fill time were optimized.

Results

Six-Month Performance

After six months of RTM production, the supplier reported the following improvements:

MetricHand Lay-upRTMChange
Monthly output150 parts600 parts+300%
Scrap rate12%5%-58%
Labor hours per part4.52.0-56%
Surface finishing time30 min8 min-73%
Part weight variation±6%±2%Improved
Thickness variation±15%±4%Improved

Finishing and Approval

The RTM parts required less post-mold finishing because both mold surfaces were smooth. The OEM approved the process change and increased the contract volume.

Key Lessons

What Worked

  • RTM pays off when monthly volume exceeds 200 to 300 parts for moderately complex shapes.
  • Proper venting is critical. Dry spots in the first month were eliminated by adding two small vents at the trailing edge.
  • Powder-bound reinforcements are preferred for RTM because they allow predictable resin flow and faster wet-out.
  • Mold heating and resin temperature control reduced cycle time variability and improved part consistency.

Conclusion

Takeaway for Automotive Suppliers

This automotive RTM case study shows that switching from hand lay-up to RTM allows suppliers to scale production without proportional labor increases. The investment was recovered through labor savings, scrap reduction, and the ability to win additional volume from the OEM.

Common Mistakes When Switching to RTM

What to Avoid

  • Underspending on mold sealing — Leaks at parting lines cause dry spots and flash.
  • Incorrect vent placement — Air must be vented at the last points to fill; missed vents create voids.
  • Using emulsion-bound mat — Powder-bound reinforcements allow faster, more predictable resin flow.
  • Skipping operator training — RTM requires discipline in clamping, injection timing, and vent monitoring.
  • Neglecting temperature control — Cold molds extend cycle time and increase variability.

Quick Decision Checklist

Process Readiness

  • Monthly volume exceeds 200–300 parts.
  • Both part surfaces require good finish.
  • Dimensional tolerance and repeatability are critical.
  • Budget includes matched mold and injection unit.
  • Powder-bound reinforcement selected.
  • Mold heating and venting designed for the resin system.
  • Operator training plan in place.

FAQ

Frequently Asked Questions

Q: Why was RTM chosen over compression molding? A: Compression molding with SMC offered fast cycles but required higher tooling investment than the projected volume justified. RTM provided a lower entry cost with sufficient quality.

Q: How long did the RTM tooling payback take? A: The supplier recovered the $40,000 tooling investment in approximately 14 months through labor and scrap savings.

Q: What reinforcement worked best in RTM? A: Powder-bound continuous filament mat and chopped strand mat were chosen for predictable resin flow and fast wet-out.

Q: What was the biggest implementation challenge? A: Proper vent placement. Adding two small vents at the trailing edge eliminated dry spots found in the first production week.

Q: Is RTM suitable for all automotive FRP parts? A: No. RTM is best for moderate volumes where both surfaces matter. Very high volumes may justify compression molding; very low volumes may remain with hand lay-up.

Data Sources and Verification

Reference Data

  • Output, scrap, and labor hour data: supplier production records during the six-month RTM evaluation period.
  • Tooling investment of $40,000: supplier budget estimate for matched aluminum molds and injection unit.
  • Resin-to-glass ratio for RTM: approximately 1.6–2.0:1 by weight for typical fiber content targets; actual value depends on reinforcement type and compaction.
  • Powder-bound vs emulsion-bound mat compatibility: powder-bound CSM is compatible with polyester, vinyl ester, and epoxy resin systems.
  • Laminate thickness guidance for hand-lay CSM: approximately 1 mm per 300 g/m²; RTM compacted laminates are typically thinner for the same glass weight.

Need Fiberglass Mat for Your Project?

We supply high-quality CSM, CFM, and specialty fiberglass products worldwide. Custom specifications available with low MOQ.

Request Free QuoteView Products

PrimeMat

Leading manufacturer of chopped strand mat and continuous filament mat for industrial applications. ISO 9001 certified with 15+ years experience.

RFQ

Request a quote

We can manufacture fiberglass mat to your exact requirements.

  • ISO 9001 certified production
  • Reply within 24 hours (EN / ZH)
  • Or WhatsApp +86 138 1403 4409

Tip: name, email, product, and quantity are enough to start a quote — add the rest only if you already know it.

Your contact details

Product requirements

Application & specific requirements