Technical guide

Biaxial Fiberglass Fabric: Double-Bias Guide

Biaxial fiberglass fabric: ±45° and 0/90° stitched double-bias construction, weights, resin savings vs CSM, applications, and buying checklist.

Biaxial fiberglass fabric
Biaxial fiberglass fabric

Biaxial fiberglass fabric guide: ±45° and 0/90° double-bias stitched fabric construction, weights in g/m² and oz/yd², resin savings vs CSM, applications, and buying checklist.

If you build laminates that carry load — hulls, blades, structural panels — the fabric you choose matters more than the resin you use. Biaxial fiberglass fabric (stitched double-bias fabric) puts straight, continuous rovings exactly where you orient them, with no woven crimp and no chopped-strand mat filler. This guide covers construction, weights, how it compares to mat-backed products such as 1708, and what to check before you order.

What Is Biaxial Fiberglass Fabric?

Biaxial fiberglass fabric is a two-layer reinforcement made from straight, unidirectional rovings laid in two directions and held together by stitching yarn — nothing else. There is no mat layer and no chemical binder. The plies are mechanically bonded by a light polyester stitching yarn, which is why this material is also called stitched fabric or non-crimp fabric (NCF).

Each ply is a set of parallel rovings, all aligned in one direction. Two plies give you two directions: typically ±45° (double bias) or 0/90° (warp and weft, aligned to the roll's length and width). Because the fibers are stitched rather than interlaced, they stay straight from roll to laminate. That is the key distinction from woven roving, where every crossover point kinks the fibers — woven crimp reduces stiffness and makes resin consumption harder to control.

The absence of a mat layer also means there is no random chopped fiber in the laminate. You decide where the glass goes, and it only goes where you orient it.

Construction and Orientation

Orientation notation tells you where the fibers point:

  • 0/90° — one ply aligned with the roll length, one across it. Best for panels and parts dominated by axial loads: flat or single-curvature laminates, bulkheads, tank walls.
  • ±45° (double bias) — both plies rotated 45° to the roll axis. Best for parts that see shear and torsion: boat hulls and decks, stringers, curved molds, and anywhere you need to wrap a corner or follow a compound curve.

Roll widths typically run about 1250–1270 mm (typical range), and custom widths from roughly 200 mm to 2600 mm are available (typical range). Stitching yarn is typically polyester; for epoxy systems, confirm epoxy-compatible sizing and stitching with your supplier before ordering — see the resin compatibility section below.

One practical note on handling: because both plies are straight rovings held only by stitching, the fabric is stable on the roll but can fray at cut edges. Cut with a sharp rotary cutter or shears, and avoid pulling plies apart at the selvage when unrolling.

Common Weights and Specifications

Biaxial fabric weight is quoted as total g/m² across both plies. The common series runs 300 / 450 / 600 / 800 / 1200 g/m², with a full available range of roughly 300–1500 g/m². For imperial buyers, 1 oz/yd² = 33.9 g/m².

Total weight (g/m²)Approx. oz/yd²OrientationNotes
425~12.5±45°~0.40 mm dry thickness (typical)
453~13.40/90°part of a standard 0/90 series
576~17±45°~0.66 mm dry thickness (typical)
601~17.70/90°part of a standard 0/90 series
855~25.20/90°~0.80 mm dry thickness (typical)
1191~35.10/90°heavy structural series
1200~35.4±45°common top-of-range product

Per-direction split example: a 425 g/m² ±45° fabric is roughly 213 + 213 g/m² per ply. Quoted weights exclude the light stitching yarn, so they reflect the glass you are actually buying.

When reading a spec sheet, check whether the weight is quoted as total laminate weight or per ply — suppliers vary, and the difference matters when you are balancing a laminate schedule. A 600 g/m² ±45° fabric, for instance, delivers 300 g/m² of glass in each diagonal direction; a 0/90° fabric of the same total weight delivers the same split along the length and width of the roll. This makes biaxial fabric straightforward to substitute into a layup that was originally designed with two unidirectional plies.

Biaxial Fabric vs 1708 (Biaxial + Mat)

1708 is a popular mat-backed product often confused with pure double bias fabric. One line of summary: a 1708-style combo mat earns its keep when you need interlaminar bonding, build-up, and a print barrier in one sheet; pure fabric wins on resin consumption, weight, drape, and directional efficiency. Full detail: 1708 fiberglass mat guide.

Pure biaxial fabric (NCF)1708 (biaxial + CSM)
ConstructionStitched roving plies, no matBiaxial roving plies + stitched chopped strand mat layer
Weight namingTotal g/m² of roving onlyNumbered name: 17 oz/yd² total, incl. ~0.8 oz/yd² mat
Best useStructural skins, weight-critical laminatesQuick build-up, bonding layers, print barrier

Biaxial vs Woven Roving vs Combo Mat

Biaxial fabricWoven rovingCombo mat
Fiber formStraight stitched rovingsInterlaced rovings (crimp)Woven roving + chopped strand mat
Resin uptakeLow (open stitch structure)Moderate–highHigher (mat layer)
Typical useStructural shear/axial laminatesGeneral-purpose thick layupsBoat hulls, fast build-up

More detail: reinforcement comparison guide, woven roving guide, combo mat.

Why No-Mat Fabric Saves Resin and Weight

Resin-to-fiber ratios by weight (all figures typical):

ReinforcementResin : glass by weight
Chopped strand mat~1.8–2.3 : 1
Woven roving~1 : 1 – 1.5 : 1
Stitched biaxial NCF~1 : 1, or slightly better

The reason is geometry. Chopped strand mat is a random fiber network — resin has to fill the space between discontinuous fibers, and mat uses powder or emulsion binder that also consumes resin. In a woven roving, crimped crossover points trap extra resin. In a stitched biaxial fabric, the fibers lie straight and the stitching creates open channels that wet out quickly, so the laminate can approach the theoretical minimum resin content for that glass weight.

Worked example: take 1 kg of glass. As CSM, it carries roughly 1.8–2.3 kg of resin. The same kilogram as biaxial fabric carries roughly 1.0–1.3 kg — a resin saving of roughly 40–50% per kg of glass at typical ratios. At equal glass weight you get a lighter laminate, and because the fibers are straight and fully aligned, a stiffer one as well.

Beyond material cost, the straight-fiber construction also gives:

  • Lower print-through — no random-fiber pattern telegraphing through gelcoat.
  • Better drape than a same-weight woven roving, especially in ±45°, which conforms to curves and corners.
  • Directional strength efficiency — strength only where you place it; you are not paying glass weight for random orientation you do not need.

Applications

  • Boat hulls and stringers — ±45° double bias for hull skins and decks in shear/torsion; 0/90° for bulkheads and panels. See our boat building applications page.
  • Wind turbine blades — large ±45° and 0/90° NCF laminates dominate spar and shell construction.
  • Structural panels — 0/90° fabric for tank walls, truck panels, and building elements; FRP tanks are a typical use.
  • Sporting goods — straight-fiber efficiency at low weight for boards, paddles, and frames.

Rule of thumb: put ±45° where the part twists or shears, and 0/90° where it bends or carries axial load.

Resin Compatibility

The glass itself is compatible with polyester, vinyl ester, and epoxy. The real constraints are the stitching yarn and the glass sizing:

  • Polyester / vinyl ester — no issues; polyester stitching and standard sizing work as-is.
  • Epoxy — confirm epoxy-compatible glass sizing and stitching yarn with your supplier. Polyester stitching can work in many epoxy systems, but verify before a structural laminate.

Unlike chopped strand mat, biaxial fabric has no powder or emulsion binder, so there is no binder-dissolution step and no styrene-solubility concern during wet-out. The open stitched structure saturates fast with any of the three resin families.

Lamination Notes

  • Cut with orientation marked. Once a ±45° ply is off the roll, you cannot tell 45° from -45° or 0° by eye. Mark the intended fiber direction on every cut piece.
  • Watch orientation deviation. Laying a ply a few degrees off its intended axis measurably reduces stiffness in the direction you designed for. Keep plies on-axis, especially in primary structure.
  • Wet-out is fast. The open stitched structure takes resin quickly — work it before it tacks to avoid dry spots or resin pooling.
  • Stack skins where needed. Pure fabric gives no interlaminar bonding layer or print barrier; add chopped strand mat or surface tissue skins where the laminate schedule calls for them.

For vacuum bagging, the open structure of stitched fabric compacts well and lets air and excess resin move through the laminate during debulk. For hand lay-up, work the resin in with a roller rather than a brush alone — the straight rovings wet out fast, but roller pressure ensures full ply-to-ply contact without voids.

Buying Checklist

Before you request a quote, confirm:

  1. Total g/m² — and the per-ply split if you need directional balance.
  2. Orientation notation — ±45° (double bias) or 0/90°.
  3. Stitch yarn type and stitch pattern — including compatibility with your resin system.
  4. Roll width and roll weight/length — standard widths run ~1250–1270 mm; custom widths roughly 200–2600 mm are available (typical).
  5. Glass sizing — matched to your resin (polyester, vinyl ester, or epoxy).
  6. MOQ and lead time — confirm per-supplier; ask for a certificate of analysis (COA) per batch.

Also worth confirming before the first order: how the fabric is packed and protected on long shipments (moisture protection matters for any stitched fabric), and whether the supplier will commit to a fixed roll length or weight tolerance so your ply-cutting plan does not drift between batches.

FAQ

What HS code does biaxial fiberglass fabric use? Under HS 2022, the old woven-fabric heading 7019.40 was deleted. Stitched (non-woven, mechanically bonded) fabrics of rovings generally classify under 7019.62 ("other closed fabrics of rovings"); genuinely woven fabrics go to 7019.61. Some jurisdictions may apply 7019.90 ("other"). Confirm with your customs broker before shipping.

Biaxial vs 1708 — which do I need? Use pure biaxial fabric when resin consumption, weight, and directional efficiency drive the design. Use 1708 when you want bonding, build-up, and a print barrier in one sheet — common in quick boat repairs and hull laminates.

Can I use epoxy with biaxial fiberglass fabric? Yes, for the glass. The constraint is sizing and stitching: confirm epoxy-compatible glass sizing and stitch yarn with your supplier before laying up a structural part.

How do I choose the weight? Match the fabric series to the laminate schedule: lighter series (300–450 g/m²) for skins and secondary structure, mid-range (600–800 g/m²) for general structural work, and heavy series (1200 g/m² and up) for primary structure. Always check the per-ply split and dry thickness against your thickness targets.

RFQ

Request a quote

PrimeMat (PrimeMat Composite Materials Co., Ltd.) manufactures chopped strand mat, continuous filament mat, surface tissue, and combo mat at an ISO 9001-certified plant in Changzhou, Jiangsu, China — supplying fiberglass reinforcement since 2009. If you need mat skins to pair with biaxial fabric, or specification advice on building a full laminate schedule, we can quote: 2-ton MOQ and 7–15 day lead time. Email csm@csm-supplier.com or WhatsApp +86 138 1403 4409.

  • ISO 9001 certified production
  • Reply within 24 hours (EN / ZH)
  • Or WhatsApp +86 138 1403 4409

Tip: name, email, product, and quantity are enough to start a quote — add the rest only if you already know it.

Your contact details

Product requirements

Application & specific requirements