Technical guide

1708 Fiberglass Mat: Stitched Biaxial CSM Explained

1708 fiberglass mat guide: learn what the numbers mean, how the stitched biaxial construction works, resin compatibility, thickness and typical applications.

1708 Fiberglass Mat: Stitched Biaxial CSM + Woven Roving Explained | PrimeMat
1708 Fiberglass Mat: Stitched Biaxial CSM + Woven Roving Explained | PrimeMat

1708 fiberglass mat guide: learn what the numbers mean, how the stitched biaxial construction works, resin compatibility, thickness and typical applications.

1708. Fiberglass Mat: Stitched Biaxial CSM + Woven Roving Explained

1708 fiberglass mat is a stitched combination reinforcement widely used in boat building, industrial tanks, and structural FRP parts. The "17" refers to the total fabric weight of 17 ounces per square yard, and the "08" refers to the 0.8 ounce per square yard chopped strand mat layer stitched to the back. It combines a 0/90° biaxial woven roving layer with a CSM layer in a single, ready-to-lay sheet.

This guide explains what 1708 fiberglass mat is, how it is constructed, how it compares to separate CSM and woven roving layers, and when to specify it. At PrimeMat, we stock 1708 fiberglass mat and custom combo mat products for marine, industrial, and transportation projects. It is written for laminators, boat builders, tank fabricators, and procurement teams sourcing reinforcements for production programs.

Key Takeaways

Quick Reference for Buyers

  • 1708 fiberglass mat is a stitched combination of 0/90° biaxial fabric and chopped strand mat, with a total weight of 17 oz/yd² (≈576 g/m²).
  • The "08" layer is approximately 0.8 oz/yd² (≈27 g/m²) of CSM on the back.
  • The stitching eliminates the need to lay CSM and woven roving separately, saving labor time and improving layer alignment.
  • 1708 provides good bidirectional strength from the biaxial layer plus bonding and build-up from the CSM layer.
  • It is compatible with polyester, vinyl ester, and epoxy resins, though the stitching thread type should be confirmed for epoxy.
  • Typical applications include boat hulls, decks, tanks, structural panels, and automotive/transportation shells.

What Does "1708" Mean?

Weight and Metric Conversion

The numbering system for stitched biaxial mats describes the total weight and the CSM backing weight in ounces per square yard:

NumberMeaningMetric Equivalent
17Total fabric weight = 17 oz/yd²≈ 576 g/m²
08CSM backing weight = 0.8 oz/yd²≈ 27 g/m²

The remaining weight, approximately 16.2 oz/yd² (≈549 g/m²), is the 0/90° biaxial woven roving layer. Some suppliers also include a light surfacing veil, which adds a small amount of weight and improves finish quality.

1708. Thickness and Areal Weight

A typical 1708 fiberglass mat has a dry thickness of approximately 0.90–1.10 mm , depending on compression and how it is measured. After wet-out and consolidation under a roller, the in-laminate thickness is usually slightly lower. The total areal weight is best verified by ASTM D3776, which measures fabric mass per unit area.

Conversion Reminder

1 oz/yd² ≈ 33.9 g/m² 17 oz/yd² × 33.9 = 576 g/m² 0.8 oz/yd² × 33.9 = 27 g/m² Always confirm the exact areal weight with your supplier, as naming conventions can vary slightly between manufacturers.

Construction of 1708 Biaxial Mat

Layers and Stitching

1708 fiberglass mat is built from three main elements:

  • 0/90° biaxial woven roving layer : Continuous glass yarns run in the 0° and 90° directions, providing strength in both warp and fill. This layer carries most of the structural load.
  • Chopped strand mat layer : Random short glass fibers are stitched to the back of the biaxial layer. This layer provides build-up, bonding between layers, and a rougher surface for interlaminar adhesion.
  • Stitching thread : Polyester or aramid thread holds the layers together through the thickness. The stitching keeps the core aligned during resin flow and cure.

The structure can be visualized as:

[0/90° biaxial woven roving] ↓ [stitching thread] ↓ [CSM backing layer] Because the layers are stitched rather than bonded with adhesive, 1708 fiberglass mat remains open and allows good resin flow during wet-out, vacuum infusion, or resin transfer molding.

Stitching Thread Types and Epoxy Compatibility

Most 1708 fiberglass mat products use polyester stitching thread, which is compatible with polyester and vinyl ester resins. For epoxy systems, verify that the stitching thread and glass sizing are epoxy-compatible. Aramid stitching is sometimes used for high-temperature or epoxy-compatible fabrics. Always confirm with the supplier when using 1708 in an epoxy laminate.

1708. vs Standard CSM vs Woven Roving Alone

Side-by-Side Performance Comparison

Feature1708 Biaxial MatStandard CSMWoven Roving Alone
Fiber orientation0/90° + randomRandom0/90°
Total weight~576 g/m²225–900 g/m²300–800 g/m²
Typical dry thickness0.90–1.10 mm0.50–2.00 mm0.30–1.20 mm
Strength directionBidirectional + some isotropicIsotropicBidirectional
Surface finishModerate (CSM side)TexturedWeave pattern
Lay-up speedFast (one layer)ModerateModerate
Labor costLowerHigher for equivalent strengthHigher
Resin consumption1.5–2.0:12.0–2.5:11.0–1.5:1
Primary useStructural skins, hulls, tanksBuild-up, cores, general laminatingPrimary structural layers

1708 is essentially a time-saving replacement for manually laying woven roving plus a layer of CSM. It provides most of the strength of the separate layers with less labor and better alignment.

The time savings come from eliminating the separate handling of two reinforcement rolls, reducing cutting operations, and ensuring the CSM layer stays in place during resin flow. In production environments, this can reduce lay-up time by 30–50% compared with manual layering.

When to Use 1708 Biaxial Mat

Boat Hulls and Decks

1708 is one of the most common reinforcements for hand-laid boat hulls and decks. The biaxial layer provides hull stiffness, while the CSM layer bonds well to the gel coat or previous laminate. It reduces the number of individual layers a laminator must place.

Industrial Tanks and Pipes

For FRP tanks and pipes requiring structural strength, 1708 builds wall thickness efficiently. The stitched construction resists layer shifting during resin flow in vacuum infusion or filament winding with added mat layers.

In tank fabrication, 1708 is often used in the structural wall layers between corrosion barriers. In pipe fabrication, it can be wrapped around mandrels or used in filament winding with chopped strand deposited between hoop windings.

Structural Panels

Large flat or curved panels benefit from the bidirectional strength and fast lay-up of 1708. It is often used in transportation, construction, and wind energy applications where panel stiffness is important.

The 0/90° fiber orientation provides good stiffness in both length and width directions, reducing the tendency of large panels to oil-can or flex under load. When combined with a foam or coremat core, 1708 creates stiff, lightweight sandwich panels.

Automotive and Transportation Panels

1708 fiberglass mat is also used in automotive body panels, truck caps, RV sidewalls, and rail interior shells. The fast lay-up and balanced strength help manufacturers hit production cycle times while meeting stiffness targets. In these applications, the CSM side is usually placed against the gel coat or primer for good bonding.

Resin Compatibility

Resin Compatibility Table

1708 is compatible with all three major fiberglass resin families, with one consideration for epoxy:

Resin TypeCompatibleNotes
Polyester✅ YesStandard choice; CSM binder dissolves in styrene
Vinyl ester✅ YesExcellent for chemical and marine applications
Epoxy✅ YesConfirm stitching thread is epoxy-compatible; use powder-bound CSM if separate

Most 1708 fiberglass mat products use polyester stitching thread, which is compatible with polyester and vinyl ester. For epoxy systems, verify with the supplier that the stitching and any sizing are epoxy-compatible. Some suppliers offer epoxy-specific stitched fabrics.

How to Laminate with 1708

Wet-Out Technique

Place the 1708 fiberglass mat layer in the mold with the CSM side facing the previous layer or gel coat. Apply resin and work it through the fabric with a brush or roller. The biaxial layer wets out more slowly than the CSM backing, so take time to ensure the entire thickness is saturated.

Use a fin or bubble roller to remove trapped air. Roll first along the stitching direction, then across it. Air trapped along the stitching lines is a common cause of voids.

Corner and Radius Handling

1708 is less conformable than plain CSM because the biaxial layer resists shear. On tight radii, cut relief slits in the fabric or use smaller pieces. For very tight corners, place a layer of standard CSM underneath the 1708 to improve conformance.

Resin Consumption

1708 fiberglass mat typically consumes 1.5–2.0:1 resin-to-fabric by weight, depending on how aggressively it is rolled. The biaxial layer uses less resin than CSM, while the CSM backing absorbs more. A 1 m² piece of 1708 fiberglass mat (576 g/m²) at a 1.7:1 ratio needs approximately 0.98 kg of resin.

Example resin calculation for 1 m² of 1708: Fabric mass = 576 g/m² Resin-to-fabric ratio = 1.7:1 Resin mass = 576 g × 1.7 = 979 g ≈ 0.98 kg/m² ## 1708 vs Other Stitched Mats ### How 1708 Compares to 1704, 1808 and DBM Specification Total Weight Construction Typical Use 1704 ~14 oz/yd² (≈474 g/m²) Biaxial + light veil Thin structural layers, lightweight panels 1708 ~17 oz/yd² (≈576 g/m²) Biaxial + 0.8 oz CSM General structural laminates, hulls, tanks 1808 ~18 oz/yd² (≈610 g/m²) Biaxial + heavier CSM Heavier structural laminates, high-load areas DBM (double bias) Varies ±45° biaxial, no CSM Torsion and shear-critical parts The right choice depends on the required thickness, strength, and weight. 1708 is the most versatile general-purpose option in this family.

1708. vs Combo Mat

Feature1708 Fiberglass MatCombo Mat
ConstructionBiaxial + CSM, stitchedMultiple skin/core/skin layers, stitched or bonded
Total weight~576 g/m² fixedVaries widely (custom)
Core includedNoOften includes coremat, foam, or balsa
Best fitStructural skins, general laminatesThick sandwich panels, fast build-up
CustomizationRoll width, stitchingCore type, layer count, width

For buyers looking for similar time-saving multi-layer products, the combo mat product page describes stitched and sandwich constructions for industrial applications. Custom specifications can often be produced with reasonable minimum order quantities.

Quality Indicators When Buying 1708

Technical Data Sheet Checklist

Not all 1708 fiberglass mat fabrics are the same. When evaluating suppliers, check the following:

Quality IndicatorWhat to Look ForWhy It Matters
Total areal weightWithin ±5% of stated 17 oz/yd² (ASTM D3776)Ensures predictable laminate thickness
CSM backing weightConsistent 0.8 oz/yd² layerAffects bonding and resin consumption
Stitch pitchEven spacing, no skipped stitchesHolds layers together during handling
Edge stabilityNo fraying or fiber lossReduces waste and handling defects
Roll width consistencyWithin stated toleranceImportant for automated cutting
Sizing / finishCompatible with target resinAffects wet-out and bond strength
Moisture contentDry, no damp smellMoisture causes weak laminates and bubbles
Tensile / tear strengthPer ASTM D5035Confirms the fabric will survive handling and pull-through

Request a technical data sheet and, if possible, a sample roll for trial before placing a large order. Burn-off testing can verify the actual glass content and layer distribution.

Sourcing 1708 and Custom Combo Mats

Customization Options and Minimum Order Quantities

1708 fiberglass mat is a standard SKU at many composite distributors, but large production programs often benefit from custom specifications. Options include:

  • Custom roll widths (1040 mm, 1270 mm, or wider)
  • Different CSM backing weights
  • Alternative stitching threads for epoxy compatibility
  • Combination with surface tissue or additional layers

For buyers looking for similar time-saving multi-layer products, the combo mat product page describes stitched and sandwich constructions for industrial applications. Custom specifications can often be produced with reasonable minimum order quantities.

Common Mistakes When Using 1708

01

Treating It Like Standard CSM

1708 fiberglass mat is thicker and stiffer than plain CSM. It requires more resin and more rolling time. Applying it with CSM techniques leads to dry spots and poor wet-out.

02

Ignoring Fiber Orientation

The warp direction of the biaxial layer should be aligned with the primary load direction. Random placement wastes the directional strength advantage.

03

Using Incompatible Stitching with Epoxy

Standard polyester stitching may not bond well with epoxy. For epoxy laminates, specify epoxy-compatible stitching or accept that the stitching may remain as a mechanical rather than chemical bond.

04

Overlapping Too Little

Because 1708 is a structural fabric, overlaps should be at least 50–75 mm to maintain strength continuity. Small overlaps create weak seams.

05

Applying Too Much Resin

Heavy saturation increases weight without adding strength. Roll firmly to achieve the target resin-to-glass ratio of 1.5–2.0:1.

What You Should Do Now

Next Steps for Buyers

If your current laminate schedule uses separate woven roving and CSM layers, evaluate whether 1708 fiberglass mat can reduce labor while maintaining performance. Test a sample panel for wet-out, strength, and surface finish before changing a production schedule.

For more background on reinforcement selection, read the guides on combo mat and CSM vs CFM vs woven roving . Conversion tables for oz/yd² and g/m² are available in the fiberglass conversion tables . When you are ready to source 1708 fiberglass mat or custom combo mats in bulk, submit your laminate schedule to PrimeMat through the quote request page .

Data Sources and Verification

Standards and Verification Notes

  • 1708 nomenclature and weights: based on North American composite industry convention for stitched biaxial fabrics.
  • Conversion 1 oz/yd² ≈ 33.9 g/m²: standard textile areal weight conversion.
  • Areal weight verification: ASTM D3776, Standard Test Method for Mass Per Unit Area (Weight) of Woven Fabric.
  • Fabric tensile/tear properties: ASTM D5035, Standard Test Method for Breaking Force and Elongation of Textile Fabrics (Strip Method).
  • Resin consumption 1.5–2.0:1 for 1708: approximate industry range based on biaxial plus CSM construction.
  • Resin compatibility: based on standard sizing and binder chemistry; confirm epoxy compatibility with supplier.
  • Applications: based on common use in marine, tank, industrial, and automotive FRP fabrication.

Need Fiberglass Mat for Your Project?

We supply high-quality CSM, CFM, and specialty fiberglass products worldwide. Custom specifications available with low MOQ.

Request Free QuoteView Products

PrimeMat

Leading manufacturer of chopped strand mat and continuous filament mat for industrial applications. ISO 9001 certified with 15+ years experience.

RFQ

Request a quote

We can manufacture fiberglass mat to your exact requirements.

  • ISO 9001 certified production
  • Reply within 24 hours (EN / ZH)
  • Or WhatsApp +86 138 1403 4409

Tip: name, email, product, and quantity are enough to start a quote — add the rest only if you already know it.

Your contact details

Product requirements

Application & specific requirements